Substance |
Formula |
Product Form |
Refractive Index |
Transmittance Range |
Evaporation
Temperature |
Application |
JS01 |
|
0.4-4.0 mm Granules, |
2.10/500nm |
360-7000nm |
2200-2300°C |
A. R. Coating,
Mutilayers |
JS02 |
|
0.4-4.0 mm Granules, |
2.35/500nm |
400-12000nm |
1800-2000°C |
A. R. Coating,
Mutilayers |
Titanium Oxide |
TiO2 |
0.4-4.0 mm Granules,
Tablets |
2.35/500nm |
400-12000nm |
2000-2200°C |
A. R. Coating,
Mutilayers |
Titanium (Ⅴ) Oxide |
Ti3O5 |
0.4-4.0 mm Granules,
Tablets |
2.35/500nm |
400-12000nm |
1800-2000°C |
A. R. Coating,
Mutilayers |
Titanium (Ⅲ)
Oxide |
Ti2O3 |
0.4-4.0 mm Granules,
Tablets |
2.35/500nm |
400-12000nm |
1800-2000°C |
A. R. Coating,
Mutilayers |
Titanium Monoxide |
TiO |
0.4-4.0 mm Granules,
Tablets |
2.35/500nm |
400-12000nm |
1700-2000°C |
A. R. Coating,
Mutilayers |
Tantalum Oxide |
Ta2O5 |
0.4-4.0 mm Granules,
Tablets |
2.10/500nm |
350-7000nm |
1900-2200°C |
A. R. Coating,
Mutilayers |
Hafnium Oxide |
HfO2 |
0.4-4.0 mm Granules,
Tablets |
1.95/500nm |
230-7000nm |
2300-2500°C |
V. V.-NIR.
Mutilayers |
Zirconium Oxide |
ZrO2 |
0.4-4.0 mm Granules,
Tablets |
2.05/500nm |
250-7000nm |
~ 2500°C |
A. R. Coating,
Mutilayers |
Niobium Oxide |
Nb2O5 |
0.4-4.0 mm Granules, |
2.30/550nm |
350-9000nm |
1800-1900°C |
A. R. Coating,
Mutilayers |
Zinc Oxide |
ZnO |
0.4-4.0mmGranules,
Tablets |
2.00/550nm |
400-16000nm |
~ 2000°C |
A. R. Coating,
Mutilayers |
Cerium Oxide |
CeO2 |
0.4-4.0 mm Granules,
Tablets |
2.20/550nm |
400-11000nm |
~ 2500°C |
A. R. Coating,
Mutilayers |
Zinc Sulfide |
ZnS |
0.4-4.0 mm Granules, Block |
2.40/550nm |
400-14000nm |
1000-1100°C |
I. R. Mutilayers |
Zinc Selenide |
ZnSe |
0.4-4.0 mm Granules, Block |
2.58/550nm |
600-15000nm |
600-900°C |
I. R. Mutilayers,
Reflection Coatings |
Ads: No. 319, Dakang Road, Baoshan District, Shanghai, P. R., Tel: 0086-21-56476657, Fax: 0086-21-56476657
Email: wu@crystaljs.com